Material Hub > Materials
Materials
-
category Aluminiumtensile strength > 211.7 MPayield strength 0,2 % > 28 MPa
-
category Aluminiumtensile strength 96 – 207 MPayield strength 0,2 % > 34 MPa
-
category Aluminiumtensile strength 170 – 304 MPayield strength 0,2 % 65 – 215 MPa
-
category Aluminiumtensile strength > 317 MPayield strength 0,2 % > 359 MPa
-
category Aluminiumtensile strength > 121.2 MPayield strength 0,2 % 41 – 305.1 MPa
-
category Aluminiumtensile strength 75 – 586 MPayield strength 0,2 % 66 – 530.8 MPa
-
category Aluminiumtensile strength –yield strength 0,2 % –
-
category Kupfertensile strength > 154.5 MPayield strength 0,2 % 54.5 – 366.7 MPa
-
category Kupfertensile strength 154.5 – 698.2 MPayield strength 0,2 % 54.5 – 366.7 MPa
-
category Kupfertensile strength 154.5 – 698.2 MPayield strength 0,2 % 54.5 – 366.7 MPa
-
category Kupfertensile strength 154.5 – 698.2 MPayield strength 0,2 % 54.5 – 366.7 MPa
-
category Kupfertensile strength 130 – 698.2 MPayield strength 0,2 % 54.5 – 366.7 MPa
-
category Kupfertensile strength 280 – 1200 MPayield strength 0,2 % > 105 MPa
-
category Kupfertensile strength 245 – 1200 MPayield strength 0,2 % 100 – 180 MPa
-
category heavy metalstensile strength –yield strength 0,2 % –
-
category heavy metalstensile strength –yield strength 0,2 % –
-
category Titantensile strength > 827 MPayield strength 0,2 % 722.6 – 1180.7 MPa