Offenzelliger Aluminiumschaum (schmelzmetallurgisches Verfahren)
Fraunhofer IWU, Abteilung Leichtbau, Textiltechnologien und Circular Economy
category zellularer Werkstoffdensity 0.16 g/cm³coefficient of linear thermal expansion 22 – 24 (10⁻⁶/K) -
category plasticsdensity 1.25 g/cm³coefficient of linear thermal expansion 110 10⁻⁶/K
-
category plasticsdensity 1.14 g/cm³coefficient of linear thermal expansion 90 10⁻⁶/K
-
category plasticsdensity 1.14 g/cm³coefficient of linear thermal expansion 90 10⁻⁶/K
-
category plasticsdensity 1.02 g/cm³coefficient of linear thermal expansion 100 10⁻⁶/K
-
category plasticsdensity 1.18 g/cm³coefficient of linear thermal expansion 80 10⁻⁶/K
-
category plasticsdensity 1.15 g/cm³coefficient of linear thermal expansion 80 10⁻⁶/K
-
category plasticsdensity 1.02 g/cm³coefficient of linear thermal expansion 100 10⁻⁶/K
-
category plasticsdensity 1.17 g/cm³coefficient of linear thermal expansion 90 10⁻⁶/K
-
category plasticsdensity 1.35 g/cm³coefficient of linear thermal expansion 60 10⁻⁶/K
-
category plasticsdensity 1.32 g/cm³coefficient of linear thermal expansion 50 10⁻⁶/K
-
category plasticsdensity 1.15 g/cm³coefficient of linear thermal expansion 80 10⁻⁶/K
-
category plasticsdensity 1.33 g/cm³coefficient of linear thermal expansion 30 10⁻⁶/K
-
category plasticsdensity 1.51 g/cm³coefficient of linear thermal expansion 30 10⁻⁶/K
-
category plasticsdensity 1.31 g/cm³coefficient of linear thermal expansion 50 10⁻⁶/K
-
category plasticsdensity 1.41 g/cm³coefficient of linear thermal expansion 50 10⁻⁶/K
-
category plasticsdensity 1.39 g/cm³coefficient of linear thermal expansion 50 10⁻⁶/K
-
category plasticsdensity 1.38 g/cm³coefficient of linear thermal expansion 50 10⁻⁶/K
-
category plasticsdensity 1.31 g/cm³coefficient of linear thermal expansion 50 10⁻⁶/K
-
category plasticsdensity 1.36 g/cm³coefficient of linear thermal expansion 50 10⁻⁶/K