  • Foamlite® P

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break > 50  %
    melting temperature 162 – 167  °C
  • SUSTAKON®

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 70  %
    melting temperature 225  °C
  • SUSTAMID® 6 ESD 60

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 8  %
    melting temperature 222  °C
  • SUSTAMID® 6 GC

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 6

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 12

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 200  %
    melting temperature 178  °C
  • SUSTAMID® 46

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 30  %
    melting temperature 295  °C
  • SUSTAMID® 66

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 12 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 15  %
    melting temperature 178  °C
  • SUSTAMID® 12 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 150  %
    melting temperature 178  °C
  • SUSTAMID® 6 GC MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 220  °C
  • SUSTAMID® 66 FG

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 260  °C
  • SUSTAMID® 66 GLD 240

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 10  %
    melting temperature 260  °C
  • SUSTAMID® 66 HS

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 20  %
    melting temperature 260  °C
  • SUSTAMID® 6G GK

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 218  °C
  • SUSTAMID® 6G HS

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 15  %
    melting temperature 216  °C

Application areas

  1. apparatus engineering
  2. filters
  3. insulation
  4. mechanical engineering
  5. orthopedics
  6. spaceflight
  7. screws
  8. tanks
  9. glazing
  10. gear wheels
  11. mechanics 108
  12. electrics 72
  13. food contact 59
  14. chemical industry 58
  15. conveyor technology 58

certificate

  1. DIBt 2

data provided by

  1. Röchling Engineering Plastics SE & Co. KG
  2. Kahmann & Ellerbrock 54
  3. Frenzelit GmbH 9
  4. Angst+Pfister GmbH 6
  5. Rhenotherm Kunststoffbeschichtungs GmbH 3
  6. igus GmbH 3
Feedback

Please feel free to give us feedback on the Material Hub.

Contact form

Usability questionnaire

QR Code