  • Foamlite® P 653 UV

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break > 50  %
    melting temperature 162 – 167  °C
  • SUSTAKON®

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 70  %
    melting temperature 225  °C
  • SUSTAMID® 6 ESD 60

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 8  %
    melting temperature 222  °C
  • SUSTAMID® 6 GC

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 6

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 12

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 200  %
    melting temperature 178  °C
  • SUSTAMID® 46

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 30  %
    melting temperature 295  °C
  • SUSTAMID® 66

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 12 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 15  %
    melting temperature 178  °C
  • SUSTAMID® 12 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 150  %
    melting temperature 178  °C
  • SUSTAMID® 6 FR

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 3  %
    melting temperature 222  °C
  • SUSTAMID® 6 GC MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 220  °C
  • SUSTAMID® 66 FG

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 260  °C
  • SUSTAMID® 66 GLD 240

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 10  %
    melting temperature 260  °C
  • SUSTAMID® 66 HS

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 20  %
    melting temperature 260  °C
  • SUSTAMID® 6G GK

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 218  °C

category

  1. metals 150
  2. plastics 124
  3. nonmetals 124
  4. organic 124
  5. synthetical 124
  6. ferrous metals 111

Application areas

  1. anvil
  2. apparatus engineering
  3. drilling
  4. power engineering
  5. automotive industry
  6. mechanical engineering
  7. paper industry
  8. spaceflight
  9. stamping
  10. mechanics 243
  11. doors and gates 117
  12. construction 105
  13. electrics 105

data provided by

  1. Key to Metals AG
  2. Röchling Engineering Plastics SE & Co. KG
  3. Kahmann & Ellerbrock 38
  4. Mittelrheinische Metallgießerei H. Beyer GmbH & Co. KG 34
  5. Wefapress Beck + Co. GmbH 7
  6. Angst+Pfister GmbH 6
Feedback

Please feel free to give us feedback on the Material Hub.

Contact form

Usability questionnaire

QR Code