  • Foamlite® P 653 UV

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break > 50  %
    melting temperature 162 – 167  °C
  • SUSTAKON®

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 70  %
    melting temperature 225  °C
  • SUSTAMID® 6 ESD 60

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 8  %
    melting temperature 222  °C
  • SUSTAMID® 6 GC

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 6

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 12

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 200  %
    melting temperature 178  °C
  • SUSTAMID® 46

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 30  %
    melting temperature 295  °C
  • SUSTAMID® 66

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 12 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 15  %
    melting temperature 178  °C
  • SUSTAMID® 12 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 150  %
    melting temperature 178  °C
  • SUSTAMID® 6 FR

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 3  %
    melting temperature 222  °C
  • SUSTAMID® 6 GC MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 220  °C
  • SUSTAMID® 66 FG

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 260  °C
  • SUSTAMID® 66 GLD 240

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 10  %
    melting temperature 260  °C
  • SUSTAMID® 66 HS

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 20  %
    melting temperature 260  °C
  • SUSTAMID® 6G GK

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 218  °C

Application areas

  1. bellows
  2. seals
  3. automotive industry
  4. semiconductors
  5. store and exhibition stand construction
  6. mechanical engineering
  7. rollers
  8. mechanics 108
  9. electrics 72
  10. food contact 59
  11. chemical industry 58
  12. conveyor technology 58

data provided by

  1. Röchling Engineering Plastics SE & Co. KG
  2. Key to Metals AG 163
  3. Kahmann & Ellerbrock 47
  4. Mittelrheinische Metallgießerei H. Beyer GmbH & Co. KG 34
  5. seal-mart GmbH 25
  6. Angst+Pfister GmbH 16
Feedback

Please feel free to give us feedback on the Material Hub.

Contact form

Usability questionnaire

QR Code