  • Foamlite® P

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break > 50  %
    melting temperature 162 – 167  °C
  • SUSTAKON®

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 70  %
    melting temperature 225  °C
  • SUSTAMID® 6 ESD 60

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 8  %
    melting temperature 222  °C
  • SUSTAMID® 6 GC

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 6

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 220  °C
  • SUSTAMID® 12

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 200  %
    melting temperature 178  °C
  • SUSTAMID® 46

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 30  %
    melting temperature 295  °C
  • SUSTAMID® 66

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 12 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 15  %
    melting temperature 178  °C
  • SUSTAMID® 12 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 150  %
    melting temperature 178  °C
  • SUSTAMID® 6 GC MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 40  %
    melting temperature 220  °C
  • SUSTAMID® 6 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 220  °C
  • SUSTAMID® 66 FG

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 GF 30

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 260  °C
  • SUSTAMID® 66 GLD 240

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 10  %
    melting temperature 260  °C
  • SUSTAMID® 66 HS

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 50  %
    melting temperature 260  °C
  • SUSTAMID® 66 MO

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 20  %
    melting temperature 260  °C
  • SUSTAMID® 6G ESD 90

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 216  °C
  • SUSTAMID® 6G GK

    Röchling Engineering Plastics SE & Co. KG

    category plastics
    tensile strain at break 5  %
    melting temperature 218  °C

Application areas

  1. covers
  2. scraper
  3. construction
  4. ventilation
  5. seals
  6. horticulture
  7. high-pressure systems
  8. interior finishing
  9. mechanical engineering
  10. sports and leisure
  11. tanks
  12. cladding
  13. packaging
  14. mechanics 108
  15. electrics 72
  16. food contact 59
  17. chemical industry 58
  18. conveyor technology 58

certificate

  1. DIBt 2

data provided by

  1. Röchling Engineering Plastics SE & Co. KG
  2. Mitsubishi Chemical Advanced Materials 67
  3. Kahmann & Ellerbrock 56
  4. seal-mart GmbH 25
  5. Angst+Pfister GmbH 16
  6. Klüber Lubrication München GmbH & Co. KG 10
Feedback

Please feel free to give us feedback on the Material Hub.

Contact form

Usability questionnaire

QR Code